Skip to content
Spezialcompounds Reference guide to engineering plastic compounds Deutsch

Tribologically modified plastics: friction and wear

Tribologically modified plastics are thermoplastics with additives such as PTFE, graphite or molybdenum disulphide that are meant to reduce friction and wear in sliding contact. Coefficient of friction and wear rate always apply to a pairing under a given load, speed and temperature. Testing follows, among others, ISO 7148-2:2026, ASTM D3702-24 and ASTM G99-23. PTFE is a fluoropolymer and is affected by the ongoing EU restriction procedure for PFAS.

Last reviewed:

At a glance

  • Coefficient of friction and wear rate describe a material pairing under defined conditions, not a material on its own.
  • The pv value is the product of contact pressure and sliding speed and limits the operating range of a sliding material.
  • Testing follows ISO 7148-2:2026, ASTM D3702-24 or ASTM G99-23; the results serve to compare pairings.
  • As internal lubricants, PTFE and graphite form a transfer film on the counterface.
  • The EU-wide restriction of PFAS has not yet been adopted: both ECHA committees gave their opinions in 2026, the Commission's proposal is pending.

Friction and wear: values of a system

Why is the coefficient of friction not a material property?

The coefficient of friction only applies to the tested pairing under the tested conditions. Different test methods can give different values for the same plastic, so method and conditions must be stated.⁠[4] For plastics the coefficient of friction often falls with increasing load and speed, until deformation and heating in the contact set a limit.⁠[4] The counterface also counts: a harder partner with asperities attacks the plastic surface.⁠[5]

What do wear rate and pv value tell you?

The specific wear rate is the volume removed, related to normal force and sliding distance, usually in mm³/(N·m).⁠[4] The pv value is the product of contact pressure p and sliding speed v. Below a critical pv value the wear rate stays roughly constant; above it, it rises sharply.⁠[4]

Which standards govern testing?

For polymer-based plain bearing materials, ISO 7148-2 applies, in its third edition since February 2026.⁠[1] ASTM D3702 in its 2024 version and ASTM G99 in its 2023 version are also widely used.⁠[2]⁠[3]

Test methods for friction and wear of plastics
MethodStandard and editionWhat is measuredNote
Testing of polymer-based plain bearing materialsISO 7148-2:2026friction and wear at defined load, sliding speed and temperature, dry and lubricatedpairings metal–polymer and polymer–polymer
Thrust washerASTM D3702-24wear rate and coefficient of friction of self-lubricating materials in rubbing contactconditions below the pv limit; run times often 50 to 4,000 hours
Pin-on-disk or ball-on-diskASTM G99-23wear and friction of a material pairingserves for ranking; deviating parameters must be stated
Sources: abstracts of the standards [1] to [3].

The texts of the standards are subject to a charge and were not available to the editors. The information comes from the public abstracts of the issuing bodies.

Sliding additives and how they work

How do PTFE and graphite work?

PTFE and graphite are added to the plastic as internal lubricants. They reduce adhesion and form a transfer film on the counterface.⁠[4] PTFE acts as a soft lubricant in a harder matrix. In graphite, the layers are only weakly bonded and shear off easily.⁠[4] For high wear resistance, the transfer film must be thin and uniform.⁠[5]

As an order of magnitude, a review gives dynamic coefficients of friction of unfilled plastics measured to ASTM D3702: from 0.10 for PTFE to 0.26 for polyamide 6.⁠[4]

Dynamic coefficients of friction of selected plasticsPTFE: 0.10; UHMW-PE: 0.12; PEEK: 0.18; PEEK with 30 % carbon fibres: 0.22; Polyamide 6: 0.26; PEEK with 30 % glass fibres: 0.31 (μ).PTFE0.10UHMW-PE0.12PEEK0.18PEEK with 30 % carbon fibres0.22Polyamide 60.26PEEK with 30 % glass fibres0.31μ
Dynamic coefficients of friction from a review, measured to ASTM D3702. The values apply only to these test conditions; not a market overview. Source: [4].
Sliding additives and reinforcements in the technical literature
AdditiveMode of actionFinding from the literatureFluorinated
PTFEsoft solid lubricant, forms transfer filmlowers friction and stick-slip in PEEKyes
Graphiteweakly bonded layers shear offwidely used solid lubricantno
Molybdenum disulphidesolid lubricantlowered the coefficient of friction of PEEK against steel by up to 30 %no
Carbon fibrescarry load, relieve the matrixPEEK with 30 %: lower wear rateno
Aramid fibresreinforcementlowered friction and wear, less than carbon fibresno
UHMW-PEsliding additive in engineering thermoplasticslow melting point of about 142 °Cno
Silicone oil, waxesincorporated lubricantsdescribed for POMno
Sources: [4] to [7]. Individual findings, not a market overview.

Does every additive lower friction and wear at the same time?

No, friction and wear can move in opposite directions. In the same review, 30 % carbon fibres raised the coefficient of friction of PEEK to 0.22 and lowered the wear rate. 30 % glass fibres raised it to 0.31 and increased the wear rate.⁠[4]

What role do UHMW-PE and silicone oil play?

Ultra-high-molecular-weight polyethylene (UHMW-PE) and silicone oil are described in patents as sliding additives for engineering thermoplastics. UHMW-PE is added to polyamide, POM, PBT or PEEK. It melts at about 142 °C, PTFE only at about 330 °C, which can set a limit under high frictional heat.⁠[6] For POM, the prior art names high-molecular-weight polyethylene, silicone oil, ultra-high-molecular-weight silicone and waxes.⁠[7]

PFAS-free: legal status and alternatives

How far has the EU restriction procedure progressed?

The restriction has been proposed and technically assessed, but not yet adopted. Authorities from Germany, the Netherlands, Denmark, Sweden and Norway submitted the proposal to the European Chemicals Agency ECHA in January 2023; it was published on 7 February 2023. It aims to restrict the manufacture, use and placing on the market of all PFAS, with exemptions where alternatives are lacking for the foreseeable future.⁠[9]⁠[12]

The Committee for Risk Assessment (RAC) adopted its opinion on 2 March 2026.⁠[11] The Committee for Socio-Economic Analysis (SEAC) has adopted its final opinion, as ECHA announced on 19 November 2026. It supports a ban with use-specific derogations and transition periods. Next, the European Commission will present a proposal on which the member states vote in the REACH Committee.⁠[12] In February 2026, this decision was expected for 2027.⁠[10]

Is PTFE covered by the restriction?

PTFE is a fluoropolymer and, by its chemical structure, falls under the definition of PFAS. The technical literature assumes that fluoropolymers are affected by the proposal. Whether they should be assessed separately is disputed there.⁠[8] Lubricants are among the sectors the committees assessed individually. Seals and machinery were added after the consultation.⁠[10] How the legal text treats fluoropolymers will only be settled with the Commission's proposal.

What does “PFAS-free” mean for sliding materials?

For sliding materials, “PFAS-free” denotes formulations without PTFE or other fluorinated additives. As the restriction has not been adopted, this procedure has so far produced no binding limit value for the claim.

As fluorine-free additives, the literature describes graphite, molybdenum disulphide, carbon fibres, aramid and UHMW-PE.⁠[5]⁠[6] In a comparison on polyimide, the combination of graphite and aramid fibres achieved lower friction and less wear than the variants with PTFE. That is a single research example, not a market overview. According to the same review, no formulation is superior under all conditions.⁠[5]

Applications and limits

Where are tribologically modified plastics used?

Tribologically modified plastics run where parts slide against each other with little or no lubricant.

  • Machinery: plain bearings and bushings, including in the mixed friction regime.⁠[4]
  • Textile machinery: sliding shoes made of carbon-fibre-reinforced PEEK that can be injection moulded.⁠[4]
  • Automotive: PEEK-based bearings in high-pressure diesel injection pumps.⁠[4]

Where are the limits?

A test rig value cannot simply be transferred to the part. ASTM D3702 leaves it to the user to judge whether the results match behaviour in service. Other test conditions can change the ranking of materials.⁠[2] ASTM G99 does not fully reproduce the lubrication, contact geometry and environment of the application.⁠[3]

  • Load: above the critical pv value, the material fails prematurely.⁠[4]
  • Harsher conditions: results from the sliding test do not automatically apply to severe abrasive wear or erosion.⁠[4]

What the material supplier needs to know

This information belongs in an enquiry:

  • Counterface: material, hardness and surface roughness
  • Contact pressure and sliding speed, and from them the pv value
  • Type of motion: rotating, oscillating or with standstill periods
  • Temperature in the contact and in the environment
  • Dry running, grease, oil or media contact
  • Permissible wear and required service life
  • PFAS requirement: PTFE permitted or fluorine-free formulation required
  • Test method for demonstrating friction and wear
  • Quantities and processing method

Frequently asked questions

What is a tribologically modified plastic?

A tribologically modified plastic is a thermoplastic with additives such as PTFE, graphite or molybdenum disulphide that is meant to show less friction and wear in sliding contact.

What is the pv value?

The pv value is the product of contact pressure and sliding speed. Above a critical pv value the wear rate rises sharply.

In which unit is the specific wear rate given?

The specific wear rate is usually given in mm³/(N·m).

Which standard applies to testing plastic plain bearing materials?

ISO 7148-2 describes the testing of polymer-based plain bearing materials and has been in its third edition since February 2026. ASTM D3702-24 and ASTM G99-23 are also widely used.

Can coefficients of friction from two data sheets be compared?

Only if test method, counterface, load, speed and temperature are the same.

How does PTFE work as a sliding additive?

PTFE is a soft solid lubricant in a harder plastic matrix. It forms a film on the counterface that lowers friction.

Is PTFE a PFAS?

PTFE is a fluoropolymer and, by its chemical structure, falls under the definition of PFAS. The technical literature sees fluoropolymers as affected by the EU restriction proposal.

Is PTFE already banned in the EU?

No. The general PFAS restriction under REACH has not been adopted. The European Commission's proposal is still pending.

Which fluorine-free sliding additives are there?

Graphite, molybdenum disulphide, carbon fibres, aramid, UHMW-PE and silicone oil are described. Whether such a formulation replaces PTFE depends on the sliding system.

Sources

All sources retrieved and checked on 23 November 2026.

  1. ISO 7148-2:2026, Plain bearings – Testing of the tribological behaviour of bearing materials – Part 2: Testing of polymer-based bearing materials. 3rd edition, February 2026. Abstract. https://www.iso.org/standard/88052.html
  2. ASTM D3702-24, Standard Test Method for Wear Rate and Coefficient of Friction of Materials in Self-Lubricated Rubbing Contact Using a Thrust Washer Testing Machine. Abstract. https://store.astm.org/d3702-24.html
  3. ASTM G99-23, Standard Test Method for Wear and Friction Testing with a Pin-on-Disk or Ball-on-Disk Apparatus. Abstract. https://store.astm.org/g0099-23.html
  4. Friedrich, K.: Polymer composites for tribological applications. Advanced Industrial and Engineering Polymer Research 1 (2018), pp. 3–39. https://doi.org/10.1016/j.aiepr.2018.05.001
  5. Panin, S. V.; Alexenko, V. O.; Buslovich, D. G.: High Performance Polymer Composites: A Role of Transfer Films in Ensuring Tribological Properties – A Review. Polymers 14 (2022), 975. https://doi.org/10.3390/polym14050975
  6. US Patent 9,181,430: Wear and friction properties of engineering thermoplastics with ultra-high molecular weight polyethylene. Description. https://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/9181430
  7. US Patent 10,479,954: Intrinsic low friction polyoxymethylene. Background section and description. https://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/10479954
  8. Améduri, B.: Fluoropolymers as Unique and Irreplaceable Materials: Challenges and Future Trends in These Specific Per or Poly-Fluoroalkyl Substances. Molecules 28 (2023), 7564. https://doi.org/10.3390/molecules28227564
  9. Umweltbundesamt (German Environment Agency): PFAS sollen EU-weit beschränkt werden (PFAS to be restricted EU-wide). News item of 7 February 2023. https://www.umweltbundesamt.de/themen/pfas-sollen-eu-weit-beschraenkt-werden
  10. European Medicines Agency (EMA): Next steps in the ECHA assessment of the PFAS universal restriction proposal under REACH. Presentation of 4 February 2026. https://www.ema.europa.eu/en/documents/presentation/presentation-next-steps-echa-assessment-pfas-universal-restriction-under-reach-l-enes-r-mezzasalma-ema_en.pdf
  11. European Chemicals Agency (ECHA): ECHA’s Risk Assessment Committee adopts its opinion on PFAS restriction proposal. Announcement, March 2026. https://www.echa.europa.eu/-/echa-s-risk-assessment-committee-adopts-its-opinion-on-pfas-restriction-proposal
  12. Farbe und Lack: ECHA befürwortet EU-weite Beschränkungen für PFAS und Chrom(VI) (ECHA supports EU-wide restrictions on PFAS and chromium(VI)). Report of 20 November 2026 on ECHA's announcement of 19 November 2026. https://www.farbeundlack.de/nachrichten/markt-branche/echa-befuerwortet-eu-weite-beschraenkungen-fuer-pfas-und-chromvi/

Related topics

This page is technical information, not advice on standards, law or design. The standards cited in their current edition and the material manufacturers' test reports are authoritative.