At a glance
- According to the literature, PPS melts at 285 °C and PEEK at 343 °C; the glass transition temperatures are 85 °C and 143 °C.
- As long-term service temperature, the literature gives about 200 °C for PPS and up to 260 °C for PEEK.
- In published tests, both polymers reached the UL 94 V-0 rating without flame retardants.
- Unreinforced PPS is brittle and is therefore almost always processed with glass or carbon fibres.
- In a published comparison, PEEK cost around eleven times as much as PPS.
PPS: polyphenylene sulphide
What is PPS?
PPS is a semi-crystalline thermoplastic whose chain consists of benzene rings linked by sulphur atoms. A review gives a glass transition temperature of 85 °C, a melting point of 285 °C and a density of 1.34 g/cm³. It is processed above 300 °C.[9] The glass transition temperature depends on the measuring method: on glass-fibre-reinforced PPS, around 120 °C was measured by dynamic mechanical analysis.[11]
Why is PPS almost always reinforced?
Unreinforced PPS is brittle. It is therefore usually mixed with glass or carbon fibres.[12] The designation GF30 or GF40 gives the glass fibre content in percent by mass. The standard ISO 20558-1 classifies PPS moulding materials by melt flow, density and tensile modulus and includes fillers and reinforcements in the designation.[2]
What mould temperature does PPS need?
The mould temperature determines how far PPS crystallises in the injection mould. In a study on PPS with 55 % glass fibres, the crystallinity index determined by X-ray diffraction rose from 18.76 % at a mould temperature of 80 °C to 36.94 % at 160 °C. Tensile strength increased from 127.29 to 140.32 MPa.[11] That is a single research example, not a market overview.
PEEK: polyetheretherketone
What is PEEK?
PEEK is a semi-crystalline thermoplastic made of phenylene rings linked by two ether groups and one ketone group.[3] The technical literature gives a glass transition temperature of 143 °C, a melting point of 343 °C and service temperatures up to 260 °C. The same review proposes 440 °C as the upper limit for processing, because decomposition products were detected from 450 °C.[10]
| Property | PPS | PEEK |
|---|---|---|
| Designation standard | ISO 20558-1:2018 | ISO 23153-1:2020 |
| Glass transition temperature | 85 °C | 143 °C |
| Melting point | 285 °C | 343 °C |
| Long-term service temperature | about 200 °C | up to 260 °C |
| Onset of decomposition | 504 °C | 570 °C |
How are PPS and PEEK designated to standard?
The abbreviations of the basic polymers are governed by ISO 1043-1. It applies in the fourth edition of 2011 with Amendment 1 of 2016 and was confirmed in 2022.[1] For PPS moulding materials ISO 20558-1:2018 applies, for PEEK moulding materials ISO 23153-1:2020. The PEEK standard classifies by melt viscosity or melt volume-flow rate, tensile modulus and tensile strength.[2][3] Both standards state that materials with the same designation do not necessarily behave the same.
The texts of the standards are subject to a charge and were not available to the editors. The information comes from the public abstracts of the issuing bodies. The text of each standard is authoritative.
What does PEEK cost compared with PPS?
PEEK is markedly more expensive than PPS. A materials selection from 2020, based on a materials database, gives around €85/kg for PEEK and €7.50/kg for PPS.[12] The prices are not current, but the ratio shows the order of magnitude.
Resistance to chemicals, water and heat
How resistant are PPS and PEEK to chemicals?
Both polymers withstand most media. Below 200 °C, PPS dissolves in almost no solvent and is resistant to acids, alkalis and salt solutions, except strongly oxidising acids.[9] For PEEK, the literature names sulphuric acid as the only solvent and a water absorption of 0.45 %.[10] According to a technical publication, PPS is highly resistant to hydrolysis.[12]
The reinforcement can be the weak point. PPS with 40 % glass fibres lost around half its tensile strength (from 153.5 to 79.6 MPa) in 30 % potassium hydroxide solution at 90 °C, because the glass fibres dissolved.[12]
ISO 175:2010 describes the immersion of unstressed test specimens in liquid chemicals and the determination of the changes in properties. Stress cracking under simultaneous mechanical load is covered by the ISO 22088 series, whose Part 3 (bent strip method) dates from 2006 and is due for revision.[4]
What do continuous use temperature and temperature index tell you?
Both values describe the temperature at which a material still retains a defined share of a property after long heat ageing. IEC 60216-1 has been in its seventh edition since December 2025; the definition of the temperature index (TI) was revised in it.[6] For the Relative Thermal Index (RTI) to UL 746B, specimens are aged without load in ovens at several temperatures. The limit is reached when the property falls below 50 % of the initial value. The TI is usually given for 5,000 and 20,000 hours.[7] General literature values such as 200 °C for PPS and 260 °C for PEEK do not replace the tested index of the individual compound.[9][10]
Fire behaviour, applications and limits
Why do PPS and PEEK burn poorly?
In both polymers, flame retardancy is a property of the chain, not an additive. Heat-resistant plastics with an aromatic backbone self-extinguish or are hard to ignite, and form a carbon-rich residue as they decompose.[8] The oxygen index to ISO 4589-2:2017 gives the lowest oxygen concentration at which a vertical specimen just continues to burn.[5]
| Property | PPS | PEEK |
|---|---|---|
| Oxygen index | 44 % | 35 % and 37.3 % |
| UL 94 | V-0 | V-0 |
| Residue after decomposition | 0.50 g/g | 0.54 g/g |
| Smoke per mass | higher | low |
UL 94 applies in the seventh edition of February 2023, last revised in July 2026.[7] What counts is the rating of the individual compound at the tested wall thickness. The two differ in smoke production: a report of the US Federal Aviation Administration counts PEEK among the polymers with low smoke, and PPS, as a sulphur-containing aromatic, among a group with higher smoke.[8]
Where are PPS and PEEK used?
- Electrical engineering and e-mobility: glass-fibre-reinforced PPS for electronics covers and capacitor housings in electric vehicles.[11]
- Automotive and aerospace: PPS compounds for parts exposed to heat and chemicals.[11]
- Medical devices: PEEK for implants in orthopaedics and spinal surgery.[10]
Where are the limits?
Three restrictions are documented in the literature:
- UV light: PPS yellows under UV radiation and loses mechanical properties.[9] PEEK fibres retained strength and modulus after 1,056 hours of UV irradiation but lost markedly in elongation at break.[10]
- Toughness: PPS without reinforcement is too brittle for load-bearing parts.[12]
- Alkalis: in hot alkali the glass fibre dissolves, not the polymer.[12]
What the material supplier needs to know
- Continuous temperature, temperature peaks and required service life
- Required temperature index (RTI or TI) with wall thickness
- Media in contact, with concentration and temperature
- Flammability rating with wall thickness, requirements for smoke density
- Stiffness, strength and impact strength; type of reinforcement
- Position of weld lines and load at these points
- Possible mould temperature and wall thicknesses
- Outdoor use or exposure to UV light
Frequently asked questions
What is the difference between PPS and PEEK?
PPS consists of benzene rings with sulphur bridges and, according to the literature, melts at 285 °C. PEEK contains ether and ketone groups, melts at 343 °C and is markedly more expensive.
What does PPS GF30 mean?
PPS GF30 denotes polyphenylene sulphide with 30 % glass fibres by mass. Unreinforced PPS is brittle, so reinforced compounds are the usual form of supply.
Up to what temperature can PPS and PEEK be used?
The technical literature gives about 200 °C for PPS and up to 260 °C for PEEK. The tested temperature index of the specific compound is binding.
Are PPS and PEEK flame-retardant without flame retardants?
Yes. In published tests both unreinforced polymers reached V-0 to UL 94. The oxygen index was 44 % for PPS and 35 to 37 % for PEEK.
Which standard governs the designation of PPS moulding materials?
ISO 20558-1:2018 sets the designation system for PPS moulding materials. For PEEK, ISO 23153-1:2020 applies, and for the polymer abbreviations ISO 1043-1:2011.
How is the chemical resistance of plastics tested?
ISO 175:2010 describes the immersion of unstressed specimens in liquid chemicals. Stress cracking under mechanical load is tested to the ISO 22088 series.
What is the difference between RTI and TI?
The Relative Thermal Index RTI is determined to UL 746B, the temperature index TI to IEC 60216. Both are based on heat ageing at several temperatures and a limit of 50 % of the initial property.
Are PPS and PEEK UV-resistant?
Only to a limited extent. PPS yellows under UV radiation and loses mechanical properties. For PEEK fibres, a study found mainly a fall in elongation at break.
Why is mould temperature important for PPS?
It determines the degree of crystallinity of the moulded part. In a study on glass-fibre-reinforced PPS, crystallinity and tensile strength rose with mould temperature between 80 and 160 °C.
Sources
All sources retrieved and checked on 23 November 2026.
- ISO 1043-1:2011, Plastics – Symbols and abbreviated terms – Part 1: Basic polymers and their special characteristics. 4th edition, November 2011, with Amd 1:2016; confirmed 2022. Abstract. https://www.iso.org/standard/50590.html
- ISO 20558-1:2018, Plastics – Poly(phenylene sulfide) (PPS) moulding and extrusion materials – Part 1: Designation system and basis for specifications. 1st edition, April 2018. Abstract. https://www.iso.org/standard/68367.html
- ISO 23153-1:2020, Plastics – Polyetheretherketone (PEEK) moulding and extrusion materials – Part 1: Designation system and basis for specifications. 1st edition, March 2020. Abstract. https://www.iso.org/standard/74746.html
- ISO 175:2010, Plastics – Methods of test for the determination of the effects of immersion in liquid chemicals. 3rd edition, October 2010; confirmed 2026. Abstract. Also ISO 22088-3:2006, Bent strip method, abstract at iso.org/standard/34874.html. https://www.iso.org/standard/55483.html
- ISO 4589-2:2017, Plastics – Determination of burning behaviour by oxygen index – Part 2: Ambient-temperature test. 2nd edition, April 2017; confirmed 2022. Abstract. https://www.iso.org/standard/60786.html
- IEC 60216-1:2025, Electrical insulating materials – Thermal endurance properties – Part 1: Ageing procedures and evaluation of test results. Edition 7.0, December 2025. Abstract. https://webstore.iec.ch/en/publication/110870
- UL Solutions: Thermal Aging Tests for Plastics. Description of heat ageing to UL 746B and IEC 60216-1. Editions according to the UL standards catalogue (shopulstandards.com): UL 746B, 5th edition 2018, last revised July 2026; UL 94, 7th edition, February 2023, last revised July 2026. https://www.ul.com/services/thermal-aging-tests-plastics
- Lyon, R. E.; Janssens, M. L.: Polymer Flammability. Report DOT/FAA/AR-05/14, Federal Aviation Administration, May 2005. https://rosap.ntl.bts.gov/view/dot/16407/dot_16407_DS1.pdf
- Gao, Y.; Zhou, X.; Zhang, M.; Lyu, L.; Li, Z.: Polyphenylene Sulfide-Based Membranes: Recent Progress and Future Perspectives. Membranes 12 (2022), 924. https://doi.org/10.3390/membranes12100924
- Zanjanijam, A. R.; Major, I.; Lyons, J. G.; Lafont, U.; Devine, D. M.: Fused Filament Fabrication of PEEK: A Review of Process-Structure-Property Relationships. Polymers 12 (2020), 1665. https://doi.org/10.3390/polym12081665
- Hong, S.-H.; Cho, B.-G.: Effect of Cooling Temperature on Crystalline Behavior of Polyphenylene Sulfide/Glass Fiber Composites. Polymers 15 (2023), 3179. https://doi.org/10.3390/polym15153179
- Zheng, X. X.; Böttger, A. J.; Jansen, K. M. B.; van Turnhout, J.; van Kranendonk, J.: Aging of Polyphenylene Sulfide-Glass Composite and Polysulfone in Highly Oxidative and Strong Alkaline Environments. Frontiers in Materials 7 (2020), 610440. https://doi.org/10.3389/fmats.2020.610440
Related topics
- High-temperature polyamides
PPA, PA9T and PA6/6T: heat resistance, water absorption and soldering. - Halogen-free flame retardancy
UL 94, Yellow Card and glow-wire tests: what the classes mean and how they are demonstrated. - Metal replacement
Stiffness, creep and temperature: when a plastic can replace a metal part. - Rail: EN 45545
Fire protection for railway vehicles: hazard levels, requirement sets and tests for plastics.
This page is technical information, not advice on standards, law or design. The standards cited in their current edition and the material manufacturers' test reports are authoritative.