Skip to content
Spezialcompounds Reference guide to engineering plastic compounds Deutsch

Metal replacement with plastics

Metal replacement means replacing an aluminium or zinc die casting with an injection moulded part made of fibre-reinforced thermoplastic. In a published measurement, polyamide 66 with 30 % glass fibres reached 9.7 GPa tensile modulus and 177 MPa tensile strength when dry; die-cast AlSi9Cu3(Fe) reached 309 MPa tensile strength. Whether the replacement works depends on sustained load, temperature, moisture and fibre orientation. Testing follows ISO 527, ISO 178 and ISO 899-1.

Last reviewed:

At a glance

  • Short-term values from tensile testing (ISO 527) and flexural testing (ISO 178) are not enough for design.
  • Under sustained load, plastic creeps; this is measured in the tensile creep test to ISO 899-1.
  • In polyamide, moisture lowers the glass transition and with it stiffness and strength.
  • The values depend on fibre direction and are lower at weld lines.
  • The heat deflection temperature HDT to ISO 75 is not a permissible continuous service temperature.

Stiffness and strength compared with die casting

How stiff and strong is a fibre-reinforced thermoplastic?

An injection moulded polyamide 66 with 30 % glass fibres by weight reached a tensile modulus of 9.7 GPa and a tensile strength of 177 MPa when dry, measured to ASTM D638.⁠[8] Tensile modulus rises almost linearly with fibre content up to 40 % by weight. Strength levels off above about 25 % by weight.⁠[7]

How does die casting compare?

Die castings of the aluminium alloy AlSi9Cu3(Fe) reached 309 MPa tensile strength, 163 MPa yield strength and 3.6 % elongation at break on 3 mm thick flat specimens. Round specimens 6 mm in diameter from the same die reached 342 MPa.⁠[9]

Tensile strength: polyamide 66 with glass fibres and aluminium die castingPA66 with 30 % glass fibres, dry: 177; Aluminium die casting, general: about 240; AlSi9Cu3(Fe), flat specimen 3 mm: 309; AlSi9Cu3(Fe), round specimen 6 mm: 342 (MPa).PA66 with 30 % glass fibres, dry177Aluminium die casting, generalabout 240AlSi9Cu3(Fe), flat specimen 3 mm309AlSi9Cu3(Fe), round specimen 6 mm342MPa
Tensile strength at room temperature from published individual measurements, not design values. Sources: [8], [9].
Published short-term values at room temperature
Material and specimenTensile strengthOther values
PA66 with 30 % glass fibres, injection moulded, dry177 MPatensile modulus 9.7 GPa
AlSi9Cu3(Fe), die cast, flat specimen 3 mm309 MPayield strength 163 MPa, elongation at break 3.6 %
AlSi9Cu3(Fe), die cast, round specimen 6 mm342 MPayield strength 168 MPa, elongation at break 5.1 %
Most aluminium die-casting alloys, as castabout 240 MPayield strength about 140 MPa, elongation at break below 1 %
Sources: polyamide after [8], aluminium after [9]. Individual measurements, not design values.

According to a materials database, the modulus of elasticity of this alloy (EN AC-46000) is 69 to 79 GPa, seven to eight times that of the polyamide named.⁠[13] For zinc die casting the editors found no freely accessible neutral source with properties. It is documented that zinc die castings age: on ZnAl4Cu1, stresses in the test fell by about 15 % through ageing at room temperature.⁠[10]

What do tensile and flexural tests tell you?

Both tests give short-term values. ISO 527-1 sets the principles of tensile testing; tensile strength and tensile modulus are determined. Part 2 governs the test conditions for moulding materials and was republished in June 2025. In it, specimens 1A and 1B were renamed A1 and A2.⁠[1] ISO 178 describes three-point bending of a freely supported bar. According to the abstract of the standard, the method is suitable for materials testing and quality control, not for determining design values.⁠[2]

Creep and relaxation under sustained load

What does creep mean for plastics?

Creep is the increase in strain under constant load. Relaxation is the reverse: with deformation held constant, stress falls over time.⁠[3]⁠[10] For glass-fibre-reinforced polyamide 6, the lifetime under load depends on the angle between load and fibre direction, on temperature and on humidity.⁠[11]

How is creep measured and presented?

The tensile creep test to ISO 899-1 loads a dumbbell specimen with constant tensile force and measures strain over time, with defined preconditioning, temperature and humidity. The data are intended for design. For this, the standard recommends tests over a wide range of stresses, times and environmental conditions.⁠[3]

As results, the standard provides for creep curves, the course of the creep modulus over time, isochronous stress–strain diagrams and creep rupture curves.⁠[3] An isochronous diagram shows stress against strain for a fixed load duration.

Temperature, moisture and thermal expansion

How do temperature and moisture affect polyamide?

Absorbed water lowers the glass transition temperature of the polyamide matrix, so moisture acts much like a higher temperature.⁠[11] An extreme case from the literature: after 24 hours in boiling water, the tensile modulus of unreinforced polyamide 66 fell by about 80 %, that of glass-fibre-reinforced grades by 45 to 65 %. Tensile strength fell by 45 to 50 %.⁠[7]

Polyamide properties therefore only apply together with the moisture state. ISO 1110 describes the accelerated conditioning of test specimens. The moisture content reached is close to equilibrium in the standard atmosphere of 23 °C and 50 % relative humidity. Without acceleration, a 4 mm thick polyamide 66 specimen would need more than a year for this.⁠[5]

The coefficient of linear thermal expansion and the glass transition temperature are determined to ISO 11359-2 by thermomechanical analysis (TMA).⁠[6]

What does the heat deflection temperature HDT tell you?

HDT is the temperature at which a test bar deflects under a defined flexural stress and heating rate. ISO 75-2 has three flexural stresses: 1.80 MPa, 0.45 MPa and 8.00 MPa. According to ISO 75-1, the results are not intended to predict behaviour in service or long-term resistance at high temperature.⁠[4] A measured example to ASTM D648: just 10 % glass fibres by weight raised the value of polyamide 66 from about 75 °C to over 245 °C.⁠[7]

Which editions of the test standards apply?

Test standards for comparing plastic and metal
PropertyStandard and editionContentStatus
Tensile propertiesISO 527-1:2019, ISO 527-2:2025tensile strength and tensile modulus; Part 2 for moulding materialsPart 1 confirmed 2025, revision scheduled
Flexural propertiesISO 178:2019flexural strength and flexural modulus6th edition, revision in draft
CreepISO 899-1:2017tensile creep test3rd edition, confirmed 2022
Heat deflection temperatureISO 75-1:2020, ISO 75-2:2013deflection temperature under flexural stressconfirmed 2026 and 2025
Moisture state of polyamideISO 1110:2019accelerated conditioning4th edition, confirmed 2024
Thermal expansionISO 11359-2:2021linear expansion and glass transition (TMA)2nd edition
Sources: abstracts of the standards [1] to [6].

The texts of the standards are subject to a charge and were not available to the editors. The information comes from the public abstracts of the issuing bodies. The text of each standard is authoritative.

Design, applications and limits

What matters in design?

Fibre orientation determines the stiffness and strength of the part, and it only arises as the mould fills.⁠[12] In injection moulded test bars the fibres lie mainly in the flow direction, so the value from the bar describes the favourable direction.⁠[7] Weld lines form where two melt fronts meet at an angle below 135°, for example with several gates. According to the literature, properties there can be up to 50 % lower.⁠[12] Gate, wall thicknesses and weld lines must therefore be agreed with the toolmaker at an early stage.

Where is metal replaced by plastic?

Examples from the cited papers, not a market overview:

  • Automotive: short-fibre-reinforced thermoplastics are used here as well as zinc die castings.⁠[10]⁠[12]
  • Electronics: here, too, the literature names short-fibre-reinforced injection moulded parts.⁠[12]
  • Machinery: zinc die castings are used in machines, glass-fibre-reinforced polyamide in semi-structural parts.⁠[7]⁠[10]

What is metal replacement not suited for?

  • Sustained load at high temperature: temperature and moisture accelerate plastic flow and shorten the lifetime under load.⁠[11]
  • Dimensional stability: glass-fibre-reinforced polyamide 66 swells differently in each direction as it absorbs moisture, because the fibres restrain the matrix along their length.⁠[8]
  • Conductivity and fire: if the part must dissipate heat, conduct electricity or meet a flammability rating, this must be clarified separately.

What the material supplier needs to know

This information belongs in an enquiry:

  • Current material with alloy, and the function of the part
  • Magnitude, direction and duration of the load
  • Continuous temperature, temperature peaks and ambient humidity
  • Permissible deformation over the service life
  • Dimensional tolerances and fits with neighbouring parts
  • Contact with media such as oil, coolant or cleaning agents
  • Wall thicknesses, flow paths and position of weld lines, where known
  • Requirements for conductivity, flammability rating and approvals
  • Quantities and functions to be integrated into the part

Frequently asked questions

What does metal replacement mean?

Metal replacement is the replacement of a metal part, for example an aluminium or zinc die casting, with an injection moulded part made of fibre-reinforced thermoplastic.

How strong is glass-fibre-reinforced polyamide compared with aluminium die casting?

In published measurements, polyamide 66 with 30 % glass fibres reached 177 MPa tensile strength when dry, die-cast AlSi9Cu3(Fe) 309 to 342 MPa depending on the specimen. These are individual measurements, not design values.

Which standard applies to tensile testing of plastics?

ISO 527-1:2019 sets the principles, ISO 527-2:2025 the test conditions for moulding materials.

Why is the flexural modulus from the data sheet not enough for design?

ISO 178 gives a short-term value. According to the abstract of the standard, the method is not suitable for determining design values.

What is an isochronous stress–strain diagram?

It shows stress against strain for a fixed load duration and is derived from creep tests to ISO 899-1.

What is the difference between creep and relaxation?

In creep the load stays the same and strain increases. In relaxation the deformation stays the same and stress decreases.

Is HDT the permissible service temperature?

No. According to ISO 75-1, the results are meant to predict neither behaviour in service nor long-term resistance.

What does conditioned mean for polyamide?

The specimen has absorbed moisture until it is close to equilibrium with the standard atmosphere of 23 °C and 50 % relative humidity. ISO 1110:2019 describes an accelerated method for this.

Why are weld lines critical in fibre-reinforced parts?

At a weld line two melt fronts meet. According to the literature, properties there can be up to 50 % lower.

Sources

All sources retrieved and checked on 23 November 2026.

  1. ISO 527-1:2019, Plastics – Determination of tensile properties – Part 1: General principles. 3rd edition, July 2019, confirmed 2025. Abstract. Also ISO 527-2:2025, Part 2: Test conditions for moulding and extrusion plastics, 3rd edition, June 2025 (iso.org/standard/85822.html). https://www.iso.org/standard/75824.html
  2. ISO 178:2019, Plastics – Determination of flexural properties. 6th edition, April 2019. Abstract. https://www.iso.org/standard/70513.html
  3. ISO 899-1:2017, Plastics – Determination of creep behaviour – Part 1: Tensile creep. 3rd edition, September 2017, confirmed 2022. Abstract and table of contents. https://www.iso.org/standard/72819.html
  4. ISO 75-1:2020, Plastics – Determination of temperature of deflection under load – Part 1: General test method. 4th edition, February 2020, confirmed 2026. Abstract. Also ISO 75-2:2013, Part 2: Plastics and ebonite, 3rd edition, April 2013, confirmed 2025 (iso.org/standard/55653.html). https://www.iso.org/standard/77576.html
  5. ISO 1110:2019, Plastics – Polyamides – Accelerated conditioning of test specimens. 4th edition, May 2019, confirmed 2024. Abstract and introduction. https://www.iso.org/standard/76395.html
  6. ISO 11359-2:2021, Plastics – Thermomechanical analysis (TMA) – Part 2: Determination of coefficient of linear thermal expansion and glass transition temperature. 2nd edition, November 2021. Abstract. https://www.iso.org/standard/81835.html
  7. Thomason, J. L.: Structure-property relationships in glass reinforced polyamide, Part 1: The effects of fibre content. Polymer Composites 27 (2006), issue 5, pp. 552–562. Author's version. https://core.ac.uk/download/9018497.pdf
  8. Thomason, J. L.: Structure-property relationships in glass reinforced polyamide, Part 3: Effects of hydrolysis ageing on the dimensional stability and performance of short glass-fibre reinforced polyamide 66. Polymer Composites 28 (2007), issue 3, pp. 344–354. https://doi.org/10.1002/pc.20312
  9. Anilchandra, A. R.; Arnberg, L.; Bonollo, F.; Fiorese, E.; Timelli, G.: Evaluating the Tensile Properties of Aluminum Foundry Alloys through Reference Castings: A Review. Materials 10 (2017), 1011. https://doi.org/10.3390/ma10091011
  10. Martinez Page, M. A.; Hartmann, S.: Modeling and Simulation of the Aging Behavior of a Zinc Die Casting Alloy. Applied Mechanics 5 (2024), pp. 646–695. https://doi.org/10.3390/applmech5040037
  11. Pastukhov, L. V.; Kanters, M. J. W.; Engels, T. A. P.; Govaert, L. E.: Influence of fiber orientation, temperature and relative humidity on the long-term performance of short glass fiber reinforced polyamide 6. Journal of Applied Polymer Science 138 (2021), 50382. https://doi.org/10.1002/app.50382
  12. Nabergoj, M.; Urevc, J.; Halilovič, M.: Modelling of Mechanical Response of Weldlines in Injection-Moulded Short Fibre-Reinforced Polymer Components. Polymers 17 (2025), 2712. https://doi.org/10.3390/polym17192712
  13. Total Materia, materials database: DIN EN AC-46000, physical properties with reference to EN 1706:2020. Data as of May 2025. https://www.totalmateria.com/en-us/material/3226613

Related topics

This page is technical information, not advice on standards, law or design. The standards cited in their current edition and the material manufacturers' test reports are authoritative.