At a glance
- Shore hardness is an empirical indentation value: scale A for softer, scale D for harder materials.
- The modulus of elasticity is determined in the tensile test to ISO 527-1:2019 and ISO 527-2:2025.
- Impact strength is tested notched or unnotched to ISO 179-1:2026 (Charpy) or ISO 180:2023 (Izod).
- Elastomer particles make polyamide impact-resistant but lower modulus and yield stress.
- Thermoplastic elastomers are divided into seven classes from TPA to TPZ under ISO 18064:2022.
Shore hardness: the value for soft materials
What does Shore hardness measure?
Shore hardness is an indentation hardness, measured with a durometer. For plastics, ISO 868 describes two types of instrument: type A for softer and type D for harder materials.[2] For vulcanised rubber and thermoplastic elastomers, ISO 48-4 applies. It also has the scales AO for very soft and AM for thin samples.[1]
ISO 48-4 was published in August 2018, replaces ISO 7619-1:2010 and was confirmed in 2024. ISO 868 still applies in the edition of March 2003, confirmed 2025.[1][2]
| Property | Standard and edition | What is measured | Note |
|---|---|---|---|
| Shore hardness, rubber and TPE | ISO 48-4:2018 | indentation hardness, scales A, D, AO, AM | replaces ISO 7619-1:2010 |
| Shore hardness, plastics | ISO 868:2003 | indentation hardness, type A or D | empirical method |
| Modulus of elasticity | ISO 527-1:2019 and ISO 527-2:2025 | tensile modulus and tensile strength | for rigid and semi-rigid materials |
| Charpy impact strength | ISO 179-1:2026 | notched and unnotched specimens | 2023 edition withdrawn |
| Izod impact strength | ISO 180:2023 | notched and unnotched specimens | state type of notch |
| Compression set | ISO 815-1:2019 | permanent deformation after compression | state temperature and duration |
| Conditioning of polyamide | ISO 1110:2019 | accelerated moisture absorption | target: close to 23 °C, 50 % relative humidity |
The texts of the standards are subject to a charge and were not available to the editors. The information comes from the public abstracts and preview pages of the publishers.
Where does Shore hardness stop being meaningful?
Shore hardness is a comparative value for control. ISO 868 calls the method empirical and states that there is no simple relationship between indentation hardness and the fundamental properties of the material.[2] According to the introduction of ISO 48-4, the reading depends on the modulus of elasticity and viscoelastic behaviour, and also on sample thickness and reading time.[1] A Shore value therefore does not replace a modulus.
Modulus: stiffness from the tensile test
How is the modulus of elasticity determined?
The modulus of elasticity of a plastic is determined in the tensile test to ISO 527 from the initial part of the stress–strain curve. Part 1 sets the principles and applies in the third edition of July 2019. ISO lists it as a standard due for revision.[3] Part 2 contains the test conditions for moulding and extrusion materials and has been in its third edition since June 2025. Specimens 1A and 1B are called A1 and A2 there.[4] The methods are intended for rigid and semi-rigid materials, including filled and reinforced compounds.[3]
Why does polyamide have a dry and a conditioned value?
Polyamide absorbs water and thereby becomes less stiff and more ductile. The water settles between the chain segments and acts as a plasticiser. In a study on PA66, dry samples contained less than 0.1 % water, at 23 °C and 50 % relative humidity about 3.0 %, after water immersion 8.2 %. The glass transition temperature fell by more than 80 K through immersion, and stiffness fell to less than a quarter.[11] That is a research example, not a market overview. ISO 1110:2019 describes accelerated conditioning of the test specimens. It aims at a moisture content close to equilibrium at 23 °C and 50 % relative humidity.[9] Only data sheet values in the same moisture state are comparable.
Impact-modified: testing and modification
Impact strength is tested to Charpy (ISO 179-1) or Izod (ISO 180). ISO 179-1 has applied in its fourth edition since March 2026, ISO 180 in its fifth of June 2023.[5][6]
What do notched and unnotched mean?
Both standards test specimens with and without a notch and evaluate the results separately. The test parameters depend on material, specimen and type of notch.[5][6]
How does an elastomer make polyamide impact-resistant?
Finely dispersed elastomer particles trigger small voids under load, and the polyamide matrix can then flow plastically instead of breaking in a brittle way. This is how a study on dry PA6 with grafted EPDM rubber describes it. Notched Izod impact strength was measured there from −40 to 80 °C. The result was a sharp transition from brittle to tough. With 6.4 % rubber by volume it lay at 31 °C, with 26.1 % by volume at about −32 °C. Smaller particles also shifted it downwards.[10] A room temperature value alone therefore does not describe an impact-modified compound.
What does toughness cost in stiffness?
The elastomer content lowers stiffness. In the same study, the modulus fell linearly with rubber content, and yield stress fell too.[10] Through the elastomer content, toughness and stiffness can therefore only be traded against each other.
TPE: thermoplastic elastomers
What is a thermoplastic elastomer?
According to the introduction of ISO 18064, thermoplastic elastomers, TPE for short, combine many characteristics of vulcanised rubber with those of thermoplastics. The standard arranges them by chemical composition into seven classes and applies in the third edition of April 2022.[7]
| Abbreviation | Class | Note |
|---|---|---|
| TPA | polyamide TPE | – |
| TPC | copolyester TPE | – |
| TPO | olefinic TPE | copolymers added in 2022 |
| TPS | styrenic TPE | – |
| TPU | urethane TPE | – |
| TPV | dynamically vulcanised TPE | vulcanised rubber phase |
| TPZ | other TPE | catch-all class |
What does compression set tell you?
Compression set shows how far a material returns to its original shape after prolonged compression. ISO 815-1:2019 describes the test for vulcanised and thermoplastic rubber at ambient or elevated temperature. The sample is held at constant deformation, usually 25 %. Tests of about 24 hours serve for specification, those of about 1,000 hours capture ageing.[8]
Where are these compounds used?
Only a few fields of use can be documented from neutral sources.
- Sealing technology: long-term compression set tests serve to estimate the service behaviour of sealing materials.[8]
- Electric vehicles and consumer electronics: a review on rubber-toughened polypropylene names a growing demand for impact-resistant materials in both sectors.[12]
- Industrial parts: polyamides are widespread in industry because of their processing and mechanical properties.[11]
What are the values not suited for?
The values are comparative values, not design data. The Shore value does not simply allow conclusions about other properties.[2] Impact values serve to estimate brittleness or toughness within the limits of the test and to compare similar materials.[5][6]
What the material supplier needs to know
- Required hardness with scale (Shore A or D) or required modulus
- Required impact strength with method, notched or unnotched
- Lowest and highest service temperature
- Moisture state in service; for polyamide dry or conditioned
- Type of load: impact, sustained load or repeated deformation
- For a sealing function: permissible compression set with temperature and duration
- Media contact, for example oils, fuels or cleaning agents
- Processing method, wall thickness and quantities
Frequently asked questions
What is the difference between Shore A and Shore D?
Shore A is used for softer, Shore D for harder materials. Both scales measure indentation hardness with a durometer.
Which standard applies to the Shore hardness of plastics?
ISO 868:2003 applies to plastics, ISO 48-4:2018 to rubber and thermoplastic elastomers.
Can the modulus be calculated from Shore hardness?
Not reliably. ISO 868 calls Shore hardness an empirical method with no simple relationship to the fundamental properties of the material.
Which standard is used to measure the modulus of plastics?
The modulus of elasticity is determined in the tensile test to ISO 527-1:2019 and ISO 527-2:2025.
What is impact-modified polyamide?
Impact-modified polyamide contains finely dispersed elastomer particles. Under load they trigger voids and allow the matrix to flow plastically.
What is the drawback of impact modification?
Modulus and yield stress fall as the elastomer content rises.
What do dry and conditioned mean for polyamide?
Conditioned denotes the state after moisture absorption, under ISO 1110 close to equilibrium at 23 °C and 50 % relative humidity.
What is a TPE compound?
A TPE compound is a thermoplastic elastomer that combines characteristics of rubber and thermoplastics. ISO 18064:2022 names the classes TPA, TPC, TPO, TPS, TPU, TPV and TPZ.
What is compression set?
Compression set states what share of a compression remains after unloading. It is tested to ISO 815-1:2019.
Sources
All sources retrieved and checked on 23 November 2026.
- ISO 48-4:2018, Rubber, vulcanized or thermoplastic – Determination of hardness – Part 4: Indentation hardness by durometer method (Shore hardness). 1st edition, August 2018, confirmed 2024. Abstract; foreword and introduction after the public preview. https://www.iso.org/standard/74969.html
- ISO 868:2003, Plastics and ebonite – Determination of indentation hardness by means of a durometer (Shore hardness). 3rd edition, March 2003, confirmed 2025. Abstract. https://www.iso.org/standard/34804.html
- ISO 527-1:2019, Plastics – Determination of tensile properties – Part 1: General principles. 3rd edition, July 2019. Abstract. https://www.iso.org/standard/527-1
- ISO 527-2:2025, Plastics – Determination of tensile properties – Part 2: Test conditions for moulding and extrusion plastics. 3rd edition, June 2025. Abstract. https://www.iso.org/standard/527-2
- ISO 179-1:2026, Plastics – Determination of Charpy impact properties – Part 1: Non-instrumented impact test. 4th edition, March 2026. Abstract. https://www.iso.org/standard/91071.html
- ISO 180:2023, Plastics – Determination of Izod impact strength. 5th edition, June 2023. Abstract; introduction after the public preview. https://www.iso.org/standard/84394.html
- ISO 18064:2022, Thermoplastic elastomers – Nomenclature and abbreviated terms. 3rd edition, April 2022. Abstract; foreword and table of contents after the public preview. https://www.iso.org/standard/80849.html
- ISO 815-1:2019, Rubber, vulcanized or thermoplastic – Determination of compression set – Part 1: At ambient or elevated temperatures. 3rd edition, November 2019, confirmed 2025. Abstract. https://www.iso.org/standard/74943.html
- ISO 1110:2019, Plastics – Polyamides – Accelerated conditioning of test specimens. 4th edition, May 2019, confirmed 2024. Abstract. https://www.iso.org/standard/76395.html
- Borggreve, R. J. M.; Gaymans, R. J.; Schuijer, J.; Ingen Housz, J. F.: Brittle-tough transition in nylon-rubber blends: effect of rubber concentration and particle size. Polymer 28 (1987), pp. 1489–1496. Full text in the University of Twente repository. https://ris.utwente.nl/ws/files/6533497/Borggreve87brittle.pdf
- Wetzel, P.; Sambale, A. K.; Uhlig, K.; Stommel, M.; Schneider, B.; Kaiser, J.-M.: Hygromechanical Behavior of Polyamide 6.6: Experiments and Modeling. Polymers 15 (2023), 3387. https://doi.org/10.3390/polym15163387
- Wee, J.-W.; Chudnovsky, A.; Choi, B.-H.: Brittle–Ductile Transitions of Rubber Toughened Polypropylene Blends: A Review. International Journal of Precision Engineering and Manufacturing-Green Technology (2023). https://doi.org/10.1007/s40684-023-00581-w
Related topics
- Metal replacement
Stiffness, creep and temperature: when a plastic can replace a metal part. - Lightweight design
Density, reinforcement and processes that make plastic parts lighter. - High-temperature polyamides
PPA, PA9T and PA6/6T: heat resistance, water absorption and soldering. - Tribology and sliding grades
Friction and wear, sliding additives and PFAS-free alternatives.